Physical Properties Metric English Comments
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group Kynar Flex® 2900 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group Kynar Flex® 3120 PVDF Copolymer  (discontinued **)
Copolymer Series, Kynar® components are used extensively in the high purity semiconductor market, the pulp and paper industry, nuclear waste processing, and the general chemical processing industry..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine J-2 PVDF Extrusion Grade
Description: J-2 PVDF is a kind of granules homopolymer, which has middle melt viscosity, J-2 is more suitable for extrusion process. J-2 PVDF pellets as raw materials, the finished products has exc..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine M-1 PVDF Molding Grade
Description: M-1 PVDF is a kind of granules homopolymer, which has high melt viscosity, M-1 is more suitable for compression molding process. M-1 PVDF pellets as raw materials, the finished products..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine T-2 PVDF for Powder Coatings
Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechani..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine Z-1 PVDF Injection Grade
Description: Z-1 PVDF is a kind of granular homopolymer, which has low melt viscosity, Z-1 is more suitable for injection molding. Z-1 PVDF pellets as raw materials, the finished products has excell..
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 3120-15 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness..
Specific Gravity 1.76 - 1.79 g/cc
1.76 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR FLEX® 3120-50 Polyvinylidene Fluoride Copolymer - Extrusion & Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Flexible, 150°C temperature rating. High stability in harsh thermal, chemical and ultraviolet environments. High toughness a..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 710, 710 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 740 Black/Red Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Pigmented. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeability, abrasion resistance; high purityAppli..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 740 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 740-02 Polyvinylidene Fluoride Homopolymer - Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. Flame and smoke suppressant. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mecha..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 760 Polyvinylidene Fluoride Homopolymer - Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. High stability in harsh thermal, chemical and ultraviolet environments. High toughness and mechanical strength, low permeabili..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Arkema Group KYNAR® 720, 720 HDP Polyvinylidene Fluoride Homopolymer- Injection Molding and Extrusion
Characteristics: Natural resin - translucent, off-white hemispheres. HDP indicates higher color stability. High stability in harsh thermal, chemical and ultraviolet environments. High toughness ..
Specific Gravity 1.73 - 1.79 g/cc
1.73 - 1.79 g/cc
Bulk Molding Compounds BMC 1401 Encapsulating Material, Electrical Grade
BMC 1401 is an electrical grade of encapsulating material characterized by a balance of soft flow and cure rate to ensure complete and proper encapsulation without voiding. Generally too soft for co..
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Shanghai Ofluorine 904 PVDF for water UF (ultrafiltration) Membranes
Description: Ofluorine 904 PVDF Powder for water UF membranes has good solubility in some special solvent, which is a good raw material for PVDF UF membranes. Ofluorine 904 PVDF as raw materials, th..