Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Shanghai Ofluorine T-2 PVDF for Powder Coatings

Category Polymer , Thermoplastic , Fluoropolymer , PVDF
Manufacturer Shanghai Ofluorine
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Shanghai Ofluorine T-2 PVDF for Powder Coatings.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: T-2 PVDF belong to thermoplastic fluorocarbon resin, which has high melt flow rate, low melt viscosity. T-2 PVDF has characteristic of chemical resistance, heat resistance, high mechanical strength, high wear resistance, anti-ultraviolet, anti-irradiation etc.Information provided by Shanghai Ofluorine Chemical Technology
Physical Properties Metric English Comments
Specific Gravity 1.77 - 1.79 g/cc
1.77 - 1.79 g/cc
ASTM D792
Bulk Density 0.200 - 0.400 g/cc
0.00723 - 0.0145 lb/in³
HG/T 2900
Water Absorption 0.10 %
0.10 %
Drying method
Melt Flow 18 - 45 g/10 min

@Load 2.16 kg,
Temperature 230 °C
18 - 45 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 75 - 76
75 - 76
ASTM D2240
Thermal Properties Metric English Comments
Melting Point 164 - 172 °C
327 - 342 °F
ASTM D3418
Descriptive Properties Value Comments
Appearance Off-white powder
Users viewing this material also viewed the following: