Polymer Property : Specific Gravity = 1.585 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.585 - 1.60 g/cc
1.585 - 1.60 g/cc
Old Hickory UltraCast Slurry PC-2000 Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
Specific Gravity 1.585 - 1.60 g/cc
1.585 - 1.60 g/cc
Old Hickory UltraCast Slurry UC-34A Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
Specific Gravity 1.585 - 1.60 g/cc
1.585 - 1.60 g/cc
Old Hickory UltraCast Slurry PC-2034 Kentucky Ball Clay
These popular slurry grades are shipped at 60% solids content and deflocculated with sodium silicate to maintain stable rheology characteristics. All the above grades are suitable for a variety of c..
Specific Gravity 1.585 g/cc
1.585 g/cc
Woven Density
Saint-Gobain COHRlastic® 3016 Low Temperature Flexibility Silicone Coated Fabric
Description: Saint Gobain Performance Plastics CHR standard COHRlastic silicone coated fabrics, available from stock, have silicone rubber dispersion coated on both sides of fiberglass. They are thi..