Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.395 g/cc | 1.395 g/cc | |
Isoflon Polyester film Polyethylene terephthalate film is a flexible film with high mechanical resistance. An excellent insulator, it preserves all its properties in a wide range of temperatures (-70°C to +150°C). .. |
|||
Specific Gravity | 1.395 g/cc | 1.395 g/cc | ISO 1183 |
Lanxess Durethan® BKV 30 H2.0 EF DUS029 901510 Nylon 6, Glass Fiber Reinforced PA 6, 30% glass fibers, injection molding, improved flowability, heat-aging stabilizedInformation provided by LANXESS. |