Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.236 g/cc | 1.236 g/cc | ISO 1183 |
Lanxess Durethan® DP 2-2240/15 H2.0 901510 Nylon 66, 15% Glass Fiber PA 66, 15% glass fibers, blow molding, heat-aging stabilized, hydrolysis stabilizedInformation provided by LANXESS. |
|||
Specific Gravity | 1.236 g/cc | 1.236 g/cc | ASTM D792 |
PolyOne Lubri-Tech™ MP-20GF/05T Modified Polyphenylene Oxide (mPPO), Glass Filled, PTFE Lubricated
(discontin Description/Features:Glass Fiber ReinforcedPTFE LubricatedPolyOne First ChoiceInformation provided by PolyOne Corporation. |