Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.15 - 1.18 g/cc | 1.15 - 1.18 g/cc | |
Nanocyl EPOCYL™ NC R1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for Hot-Melt Formulation Purposes: Dilution Factor 6 EPOCYL™ NC R1MY-02 is a Master Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl, with a suggested dilution factor of 6. .. |
|||
Specific Gravity | 1.15 - 1.18 g/cc | 1.15 - 1.18 g/cc | |
Nanocyl EPOCYL™ NC R1MY-04 Master Batch Liquid tetrafunctional epoxy Resin for solvent based Formulation Purposes: Dilution Factor 6 EPOCYL™ NC R1MY-04 is a Master Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl with a suggested dilution factor of 6. .. |
|||
Specific Gravity | 1.15 - 1.18 g/cc | 1.15 - 1.18 g/cc | |
Nanocyl EPOCYL™ NC E1MY-02 Master Batch Liquid tetrafunctional epoxy Resin for non-Solvent Formulation Purposes EPOCYL™ NC E1MY-02 is a Mater Batch based on liquid tetrafunctional epoxy resin containing high concentration of Carbon Nanotubes (CNT) produced by Nanocyl. It is specifically developed to enhance.. |
|||
Specific Gravity | 1.12 - 1.18 g/cc | 1.12 - 1.18 g/cc | ASTM D 792 |
Karina 4000/35-IE MBPEBD Green Color Concentrate Color concentrate recommended for polyolefin applications and 2% minimum adding.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.12 - 1.18 g/cc | 1.12 - 1.18 g/cc | ASTM D 792 |
Karina E 1000/00856-IE MBPEB White Mineral concentrate, recommended for polyolefinics applications (films/bags). Usage estimated from 10% to 20%.Information provided by Karina Indústria e Comércio de Plásticos Ltda. |
|||
Specific Gravity | 1.14 - 1.18 g/cc | 1.14 - 1.18 g/cc | ASTM D-792 |
Axiall 8554 Moldings & Extrusions Flexible PVC General purpose, jelly clear flexible PVC compound recommended for extrusion or molding applications.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Specific Gravity | 1.14 - 1.18 g/cc | 1.14 - 1.18 g/cc | ASTM D792 |
Compuestos Dominicanos Polycom CH-550140 PVC Compound Compuestos Dominicanos SA produces a wide variety of PVC compounds for the injection molding of footwear products; everything from full injection, shoe soles, boots, and PVC compounds for oil resist.. |