Polymer Property : Specific Gravity = 1.147 g/cc
Polymer Property :
Specific Gravity =
1.147 g/cc
Product List
Physical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties
Metric
English
Comments
Specific Gravity
1.147
g/cc
1.147
g/cc
ISO 1183
Stir SpA POROCELL Z 545 ATS (PVC)