Polymer Property : Specific Gravity = 1.147 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 1.147 g/cc
1.147 g/cc
ISO 1183
Stir SpA POROCELL Z 545 ATS (PVC)
Application: Matt super foam for injection moldingInformation provided by STIR SpA