Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.119 g/cc @Temperature 25.0 °C |
1.119 g/cc @Temperature 77.0 °F |
|
Dow Corning SILASTIC® LC-30-2004 PART A&B KIT 30 Durometer, 2 parts, 1 to 1 mix, translucent, FDA 21 CFR 177.2600 and BfR, XV, molding and injection molding grade Liquid Silicone Rubber.Information provided by Dow Corning |
|||
Specific Gravity | 1.119 g/cc | 1.119 g/cc | mixed, uncured |
Atom Adhesives AA-BOND FDA2T Epoxy Adhesive AA-BOND FDA2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received .. |