Material Notes:
AA-BOND FDA2T is a thixotropic epoxy resin system specifically developed for medical device applications. It has been tested in accordance with USP biological reactivity tests, in vivo and received Class VI approval. AA-BOND FDA2T is an effective electrical insulator, and it provides low permeability to gases and vapors and good resistance to water, weather, lubricants and fuels, to mild acids and alkalis, and many other organic and inorganic compounds.Appearance: AmberCure Type: Heat cure or Room TemperatureBenefits:Medium viscosityElectrically InsulatingLow permeability to gases and vaporsLow temperature cure Mix Ratio by weight: 100:93/Resin:HardenerTypical Application: Medical, Food preparation processing and packagingInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Specific Gravity 1.119 g/cc
1.119 g/cc
mixed, uncured
Solids Content 100 %
100 %
reactive, uncured
Viscosity 24000 - 26000 cP
24000 - 26000 cP
uncured
Mechanical Properties Metric English Comments
Hardness, Shore D 79
79
cured
Elongation at Yield 9.0 %
9.0 %
Adhesive Bond Strength 12.4 MPa
1800 psi
cured
Thermal Properties Metric English Comments
CTE, linear 52.9 µm/m-°C
29.4 µin/in-°F
Maximum Service Temperature, Air 145 °C
293 °F
Minimum Service Temperature, Air -70.0 °C
-94.0 °F
Glass Transition Temp, Tg 70.0 °C
158 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.20e+14 ohm-cm
1.20e+14 ohm-cm
Dielectric Constant 3.4

@Frequency 1000 Hz
3.4

@Frequency 1000 Hz
Dielectric Strength 16.5 kV/mm
420 kV/in
Dissipation Factor 0.020

@Frequency 1000 Hz
0.020

@Frequency 1000 Hz
Processing Properties Metric English Comments
Cure Time 60.0 - 240 min

@Temperature 65.0 °C
1.00 - 4.00 hour

@Temperature 149 °F
1440 min

@Temperature 25.0 °C
24.0 hour

@Temperature 77.0 °F
Pot Life 180 min
180 min
uncured