Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.0867 g/cc @Temperature 25.0 °C |
1.0867 g/cc @Temperature 77.0 °F |
|
Dow Corning 2-2078 FLUID A liquid amino phenyl silicone resin primarily for use in hair care products, but has utility in color cosmetics as well.Information provided by Dow Corning |