Dow Corning 2-2078 FLUID

Category Fluid
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 2-2078 FLUID.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A liquid amino phenyl silicone resin primarily for use in hair care products, but has utility in color cosmetics as well.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.0867 g/cc

@Temperature 25.0 °C
1.0867 g/cc

@Temperature 77.0 °F
Viscosity 1000 - 3000 cP
1000 - 3000 cP
dynamic
Optical Properties Metric English Comments
Refractive Index 1.49 - 1.51
1.49 - 1.51
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Active Content (%) 100
Appearance colorless
Color pale yellow