Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.037 g/cc @Temperature 25.0 °C |
1.037 g/cc @Temperature 77.0 °F |
|
Dow Corning 19 ADDITIVE DOW CORNING 19 Additive is a modified silicone, designed primarily to provide levelling, slip and mar resistance in water and solvent borne paints, inks and coatings. This additive also improves ant.. |
|||
Specific Gravity | 1.037 g/cc | 1.037 g/cc | |
Dow Corning 190 Fluid Dow Corning® 190 Fluid is a silicone glycol copolymer.Information provided by Dow Corning |