Material Notes:
DOW CORNING 19 Additive is a modified silicone, designed primarily to provide levelling, slip and mar resistance in water and solvent borne paints, inks and coatings. This additive also improves anti blocking properties, gloss and substrate wetting.Information provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.037 g/cc

@Temperature 25.0 °C
1.037 g/cc

@Temperature 77.0 °F
Thermal Properties Metric English Comments
Flash Point 63.0 °C
145 °F
closed cup
Processing Properties Metric English Comments
Shelf Life 18.0 Month
18.0 Month
Descriptive Properties Value Comments
Active Content (%) 100