Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 1.023 g/cc | 1.023 g/cc | |
Northstar Polymers PPB-023 Curing Agent Information provided by Northstar Polymers. |
|||
Specific Gravity | 1.023 g/cc | 1.023 g/cc | 20/20°C |
LyondellBasell Glycol Ether DM Diethylene glycol methyl ether Information provided by Lyondell. |
|||
Specific Gravity | 1.023 g/cc | 1.023 g/cc | |
Struktol V-HRW LUBRICANT ADDITIVE FOR PVC AND POLYMER PROCESSING Applications: STRUKTOL® V-HRW is a highly compatible, rigid PVC lubricant with both internal and external properties. It is particularly useful in clear PVC articles due to its excellent clarity .. |