Information provided by Lyondell.
Physical Properties Metric English Comments
Specific Gravity 1.023 g/cc
1.023 g/cc
20/20°C
Density 1.02 g/cc

@Temperature 20.0 °C
0.0368 lb/in³

@Temperature 68.0 °F
Solubility in Water 100 %
100 %
20°C
Viscosity 3.9 cP

@Temperature 25.0 °C
3.9 cP

@Temperature 77.0 °F
Molecular Weight 120.15 g/mol
120.15 g/mol
Vapor Pressure 0.000267 bar

@Temperature 20.0 °C
0.200 torr

@Temperature 68.0 °F
Evaporation Loss 2.0 %
2.0 %
n-BuAc=100%
Surface Tension 34.8 dynes/cm
34.8 dynes/cm
25°C
Thermal Properties Metric English Comments
Boiling Point 194 °C
381 °F
at 760 mmHg
Flash Point 84.0 °C
183 °F
Tag Closed Cup
Optical Properties Metric English Comments
Refractive Index 1.4268

@Temperature 25.0 °C
1.4268

@Temperature 77.0 °F