Physical Properties Metric English Comments
Specific Gravity 0.996 g/cc
0.996 g/cc
25°C; ASTM D4052
ExxonMobil Exxon Hyjet IV-A
Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the per..
Specific Gravity 0.996 g/cc
0.996 g/cc
25°C; ASTM D4052
ExxonMobil Exxon Hyjet IV-A
Exxon HyJet IV-Aplus is a fire-resistant phosphate ester hydraulic fluid designed for use in commercial aircraft. It is the best-performing Type IV fluid and offers to a great extent many of the per..
Specific Gravity 0.996 g/cc
0.996 g/cc
Esstech X-887-7424 1,6-Hexanediol Dimethacrylate, C14H22O4
1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Tox..
Specific Gravity 0.996 g/cc
0.996 g/cc
Esstech X-887-7446 1,6-Hexanediol Dimethacrylate, C14H22O4
1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Tox..
Specific Gravity 0.996 g/cc
0.996 g/cc
Esstech X-887-7466 1,6-Hexanediol Dimethacrylate, C14H22O4
1, 6 - Hexanediol dimethacrylate or HDDMA is a hydrophobic dimethacrylate. It assists with cross-linking and can be used in sealants, adhesives, inks and electronic photopolymers. Listed on the Tox..