Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
LG Chemical LUTENE-H BE0400 HDPE Description: LUTENE - H BE0400 is an excellent materials for blow-molded articles with high density and rigidity. It has good flow characteristics and impact resistance.Applications: Blow molded con.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | |
Teknor Apex TruVis Esters™ TTDTM Tri-Tridecyl Trimellitate |
|||
Specific Gravity | 0.957 - 0.965 g/cc @Temperature 20.0 °C |
0.957 - 0.965 g/cc @Temperature 68.0 °F |
|
The Chemical Company ChemFlexx™ 911P Alkyl Phthalate ChemFlexx™ is a slightly odorous linear plasticizer with outstanding performance properties. It has superior low temperature flexibility, low volatility and foggin, and excellent oven-aged retaine.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
A. Schulman POLYFORT™ FPP 1512E Talc Filled, High Impact Copolymer Polypropylene DescriptionPolyfort® FPP 1512E is a 10% talc-filled, high impact copolymer polypropylene. ApplicationPolyfort® FPP 1512E is suitable for extrusion or blow molding applications. Information provid.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ISO 1183 |
Total HDPE 5802 High Density Polyethylene - Blow Molding HDPE 5802 is a high density polyethylene with excellent compromise between stiffness and Environmental Stress Crack Resistance. It has been specifically designed for the manufacture of blow molded .. |
|||
Specific Gravity | 0.957 g/cc @Temperature 25.0 °C |
0.957 g/cc @Temperature 77.0 °F |
|
Dow Corning XIAMETER® PMCPPMX-0345 Cyclosiloxane Blend Is chemically equivalent to DOW CORNING® 345 FLUID. A blend of polydimethylcyclosiloxanes composed mainly of cyclopentasiloxane and cyclohexasiloxane for use in skincare, suncare, color cosmetics, .. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D792 |
Entec Hypel® PEHD4/.955 HDPE Available in North America Features: Food Contact Acceptable and High DensityAgency Ratings: FDA 21 CFR 177.1520RoHS Compliant Form: Pellets Information provided by Entec |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D1505/D792 |
Braskem JV060U Injection Molding High Density Polyethylene Boxes for beverages bottles; Boxes in general; Technical parts.Information provided by Braskem. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | |
Radici Radilene® R 70 IE 5058 B High Density Polyethylene Shore hardness: 64 D (3s)Processable, recyclable, no charge and completely non-toxicApplication examples: coating of corrugated and non-corrugated pipe (conduit, plumbing pipe, steel pipe coating a.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D1505 |
Chevron Phillips Marlex® 9515H High Density Polyethylene, Blow Molding This gas phase, high molecular weight, hexane copolymer with antistatic agent is tailored for lightweight blow molded applications that:Require excellent stiffness to ESCR ratioRequire good melt str.. |
|||
Specific Gravity | 0.957 g/cc | 0.957 g/cc | ASTM D1505 |
LG Chemical LUTENE-H ME8000 HDPE Description: LUTENE-H ME8000 is mainly intended for injection molding of containers. It has good mechanical properties and high productivity.Applications: Silicone cartridge, containers, complicated.. |