Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.947 - 0.953 g/cc @Temperature 25.0 °C |
0.947 - 0.953 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne reFlex™ 100 Plasticizer, Bio-derived Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 94% biobased.Information provided by PolyOne |