Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.947 - 0.953 g/cc @Temperature 25.0 °C |
0.947 - 0.953 g/cc @Temperature 77.0 °F |
ASTM D4052 |
PolyOne reFlex™ 100 Plasticizer, Bio-derived Bio-derived, non-phthalate plasticizer; USDA BioPreferred® certified 94% biobased.Information provided by PolyOne |
|||
Specific Gravity | 0.947 g/cc | 0.947 g/cc | ASTM D792 |
Network Polymers Softflex® 0826 Description: Softflex® Thermoplastic Elastomer AlloyInformation provided by Network Polymers Inc. |
|||
Specific Gravity | 0.947 g/cc | 0.947 g/cc | ASTM D792 |
Teknor Apex Sinpolene TPP2010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Automotive Applications; Housings Forms: Pellets Process.. |
|||
Specific Gravity | 0.947 g/cc | 0.947 g/cc | ISO 1183 |
Total Lumicene® mPE M 4707 EP Metallocene Polyethylene, Blown Film This product is a Total Ecosolutions grade.Lumicene® mPE M 4707 EP is a second generation metallocene based High Density Polyethylene with hexene as comonomer.Lumicene® mPE M 4707 EP can be proces.. |