Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.896 - 0.901 g/cc | 0.896 - 0.901 g/cc | Hydrometer; ASTM D1298 |
LG Chemical Butyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |