Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.896 - 0.901 g/cc | 0.896 - 0.901 g/cc | Hydrometer; ASTM D1298 |
LG Chemical Butyl Acrylate Features: Low Color - Refining process are improved for produce the low color. Color is the main quality factor that influence the property of the final products. Low Acidity - Through the multistag.. |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | at 80°C |
Struktol CARSTAB® DLTDP Thioester Antioxidant Thioester synergist that is particularly effective as a long term heat aging stabilizer when used in conjunction with primary antioxidants.CARSTAB DLTDP is especially recommended to protect high den.. |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | 15°C |
ExxonMobil 312 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Mobil Pegasus 710 40 Mobil Pegasus 710 is a premium performance gas engine oil primarily intended for the lubrication of modern high-speed four-cycle engines where oil consumption is very low. These engines are generall.. |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 320 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | 15°C |
ExxonMobil 312 Mobilgard 12 Series Mobilgard 12 Series by ExxonMobil are high performance diesel engine oils developed for use in trunk piston engines operating on low sulphur distillate fuels in marine and industrial applications. T.. |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 320 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Specific Gravity | 0.896 g/cc @Temperature 25.0 °C |
0.896 g/cc @Temperature 77.0 °F |
|
Dow Corning 5200 Formulation Aid An alkylmethyl siloxane copolyol designed to prepare stable water-in-oil emulsions.Information provided by Dow Corning |
|||
Specific Gravity | 0.896 g/cc | 0.896 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Mobil Pegasus 710 40 Mobil Pegasus 710 is a premium performance gas engine oil primarily intended for the lubrication of modern high-speed four-cycle engines where oil consumption is very low. These engines are generall.. |