Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.887 g/cc | 0.887 g/cc | ISO 1183 |
Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene Clearflex CH G0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has an excellent compatibility with polyolefins and fillers.Main Applic.. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 20/20°C |
LyondellBasell PNP Propylene glycol normal propyl ether Information provided by Lyondell. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil Vactra 3 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 100 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil 27 Mobil DTE 20 Series Mobil DTE 20 Series oils are supreme performance anti-wear hydraulic oils designed to satisfy a wide range of hydraulic equipment requirements. They provide long oil/filter life and optimum equipmen.. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil 27 Mobil DTE 20 Series Mobil DTE 20 Series oils are supreme performance anti-wear hydraulic oils designed to satisfy a wide range of hydraulic equipment requirements. They provide long oil/filter life and optimum equipmen.. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 15°C; ASTM D1298 |
ExxonMobil Mobil Vactra 3 The Mobil Vactra Oil Numbered Series are premium-quality lubricants specifically designed to fully meet the requirements for accuracy and parts finish of todays high production machine tools. They a.. |
|||
Specific Gravity | 0.887 g/cc | 0.887 g/cc | 15.6°C; ASTM D1298 |
ExxonMobil Teresstic 100 TERESSTIC is the brand name for a line of long-service-life lubricating oils that have ranked for over five decades among the finest products of their kind. Continually improved over the years, TERE.. |