Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , LDPE , Very Low Density Polyethylene (VLDPE)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Clearflex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Clearflex® CH G0 Very Low Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Clearflex CH G0 is a linear low density polyethylene, with antioxidants, characterized by a very low density (VLDPE).The resin has an excellent compatibility with polyolefins and fillers.Main Applications: Clearflex CH G0 is recommended for applications in which soft touch and flexibility are required, for improvement of impact resistance when used as additive in blend with other polyolefins formulated with or without mineral fillers.Information provided by Polimeri Europa.
Physical Properties Metric English Comments
Specific Gravity 0.887 g/cc
0.887 g/cc
ISO 1183
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 190 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ISO 1133
Mechanical Properties Metric English Comments
Film Elongation at Break, MD >= 800 %
>= 800 %
ISO 527-3
Film Tensile Strength at Break, MD 13.0 MPa
1890 psi
ISO 527-3
Thermal Properties Metric English Comments
Melting Point 110 °C
230 °F
Internal method
Vicat Softening Point 38.0 °C

@Load 1.00 kg
100 °F

@Load 2.20 lb
ISO 306/A
Brittleness Temperature <= -70.0 °C
<= -94.0 °F
ASTM D746
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
clear; thickness not quantified