Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.400 - 0.500 g/cc | 0.400 - 0.500 g/cc | ASTM D-792 |
Axiall 3801 Vinyl Foam, Extrusion Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall.. |