Polymer Property : Specific Gravity = 0.400 g/cc Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Specific Gravity 0.400 - 0.500 g/cc
0.400 - 0.500 g/cc
ASTM D-792
Axiall 3801 Vinyl Foam, Extrusion
Georgia Gulf 3801, 3802, and 3803 are vinyl foam compounds designed for applications requiring lower density than standard rigid vinyls.Information provided by Georgia GulfGeorgia Gulf became Axiall..