Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.300 - 0.360 g/cc | 0.300 - 0.360 g/cc | |
Dow Corning 3-8159 RF SILICONE FOAM KIT Two-part, room temperature curing silicone foam system, 1:1 Ratio, Addition CureInformation provided by Dow Corning |