Dow Corning 3-8159 RF SILICONE FOAM KIT

Category Polymer , Adhesive , Thermoset , Silicone , Silicone Foam
Manufacturer Dow Corning
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Dow Corning 3-8159 RF SILICONE FOAM KIT.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Two-part, room temperature curing silicone foam system, 1:1 Ratio, Addition CureInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 0.300 - 0.360 g/cc
0.300 - 0.360 g/cc
Mechanical Properties Metric English Comments
Hardness, Shore OO 65 - 70
65 - 70
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Color Colorless
Part B
Grey
Part A
Flowable yes
Working Time (min) 3