Physical Properties | Metric | English | Comments |
---|---|---|---|
Brookfield Viscosity | 0.89 cP @Temperature 25.0 °C |
0.89 cP @Temperature 77.0 °F |
M1433B; typical of water thin materials; ASTM D2196-86; LVT |
Lord Adhesives Aeroglaze® M1433 Elastomeric Polyurethane Rain Erosion Coating Aeroglaze® M1433 elastomeric coating functions exceptionally well in abrasive environments. Inherent flexibility, corrosion resistance, and energy absorptive properties make Aeroglaze M1433 elast.. |
|||
Brookfield Viscosity | 0.89 cP @Temperature 25.0 °C |
0.89 cP @Temperature 77.0 °F |
Part B, M201; LVT, Spindle #4 @ 30rpm |
Lord Adhesives Chemglaze® M331 Elastomeric Polyurethane Chemglaze® M331 is a two package, ASTM D-16 Type IV elastomeric polyurethane coating. Cured films produced from this coating are tough, flexible, and resistant to erosion, abrasion, and impact. T.. |