Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 63.5 - 94.0 cm | 25.0 - 37.0 in | Average value: 83.0 cm Grade Count:6 |
Overview of materials for PVC, Molded This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb.. |