Polymer Property : Spiral Flow = 37.0 in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 63.5 - 94.0 cm
25.0 - 37.0 in
Average value: 83.0 cm Grade Count:6
Overview of materials for PVC, Molded
This property data is a summary of similar materials in the MatWeb database for the category "PVC, Molded". Each property range of values reported is minimum and maximum values of appropriate MatWeb..