Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 220 cm @Thickness 1.00 mm |
86.6 in @Thickness 0.0394 in |
365°C nozzle, 160°C tool |
Victrex® PEEK 150G903 Black Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, easy flow, FDA food contact compliant, colou.. |