Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 0.800 - 77.0 cm | 0.315 - 30.3 in | Average value: 51.6 cm Grade Count:3 |
Overview of materials for Nylon 66, Impact Grade This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Impact Grade". Each property range of values reported is minimum and maximum values of appropr.. |