Physical Properties | Metric | English | Comments |
---|---|---|---|
Spiral Flow | 34.0 - 50.0 cm | 13.4 - 19.7 in | Average value: 43.8 cm Grade Count:12 |
Overview of materials for Nylon 6, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. E.. |