Physical Properties Metric English Comments
Spiral Flow 73.7 cm
29.0 in
PolyOne Geon™ Vinyl Rigid Molding MR840 Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne
Spiral Flow 73.7 cm
29.0 in
PolyOne Geon™ HTX M6230 Polyvinyl Chloride Alloy (PVC Alloy)
Information provided by PolyOne
Spiral Flow 73.7 cm
29.0 in
PolyOne Geon™ Vinyl Rigid Molding M4910 (USP CLASS VI for TRANS 9494 only) Polyvinyl Chloride, Rigid (PVC, Rigid)
Information provided by PolyOne