Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Spiral Flow = 2.60 cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Spiral Flow 2.60 cm
1.02 in
Tipco Tipcolite® TPF 1119 - Latex Modified Phenolic Resin having 26 mm Norton Flow with 9% Hexamine
Latex Modified Phenolic Resin having 26mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: BrakeliningInformation provided by the Manufacturer, Tipco Industries Ltd., Indi..
Copyright © lookpolymers.com All Rights Reserved