Tipco Tipcolite® TPF 1119 - Latex Modified Phenolic Resin having 26 mm Norton Flow with 9% Hexamine

Category Polymer , Thermoset , Phenolic
Manufacturer Tipco Industries Ltd., India
Trade Name Tipcolite®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Tipco Tipcolite® TPF 1119 - Latex Modified Phenolic Resin having 26 mm Norton Flow with 9% Hexamine.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Latex Modified Phenolic Resin having 26mm Norton Flow, in Powder FormApplications: Automotive & IndustrialProcessing: BrakeliningInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Physical Properties Metric English Comments
Spiral Flow 2.60 cm
1.02 in
Thermal Properties Metric English Comments
Melting Point 86.0 °C
187 °F
TRN-14