Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm
0.020 - 0.040 in/in
ASTM D955
PolyOne LubriOne™ ATH-000/04S Acetal (POM) Homopolymer
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm
0.020 - 0.040 in/in
ASTM D955
PolyOne LubriOne™ SF-30CF/15T Polyphenylene Sulfide (PPS)
LubriOne™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. L..
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm

@Thickness 3.18 mm
0.020 - 0.040 in/in

@Thickness 0.125 in
ASTM D955
PolyOne Stat-Tech™ NN-40CF/000 FRV0 Natural Polyamide 66 (Nylon 66)
Information provided by PolyOne
Linear Mold Shrinkage, Flow 0.036 - 0.040 cm/cm
0.036 - 0.040 in/in
ASTM D955
PolyOne Versaflex™ CL2000X Thermoplastic Elastomer (TPE)
Versaflex™ CL2000X is an ultra-soft TPE designed for use in injection molding applications where exceptional clarity and an extremely soft feel are desired. - Tactile Feel - Ultra-Soft - Water Clar..
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm

@Thickness 3.18 mm
0.020 - 0.040 in/in

@Thickness 0.125 in
ASTM D955
PolyOne Edgetek® NN-40CF/000 FRV0 NATURAL Polyamide 66 (Nylon 66)
The Edgetek® Engineering Thermoplastic Compounds portfolio covers a broad range of standard and custom-formulated high performance materials. This portfolio includes high-temperature materials for ..
Linear Mold Shrinkage, Flow 0.0070 - 0.040 cm/cm
0.0070 - 0.040 in/in
ISO 294-4
Polyplastic Armlen® PP MF 30-3IM Polypropylene, 30% Mineral Filled
UV resistant, impact modified, heat stabilizedInformation provided by PolyPlastic Group.
Linear Mold Shrinkage, Flow 0.025 - 0.040 cm/cm

@Time 86400 sec
0.025 - 0.040 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP LUBRICOMP KL004L Acetal Copoly (Asia Pacific)
LNP* Lubricomp* KL004L is a compound based on Acetal Copolymer resin containing PTFE. Added features of this material include: Internally Lubricated, Low Extractible.
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Lubricomp RL001 PA 66
LNP Lubricomp* RL001 is a Nylon 6/6 base resin containing PTFE lubricant. Characteristics are internally lubricated.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.010 - 0.040 cm/cm

@Time 86400 sec
0.010 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp KB004 Acetal Copolymer
LNP THERMOCOMP* KB004 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.010 - 0.040 cm/cm

@Time 86400 sec
0.010 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp WB006 PBT
LNP* Thermocomp* WB006 is a compound based on Polybutylene Terephalate resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Linear Mold Shrinkage, Flow 0.020 - 0.040 cm/cm

@Time 86400 sec
0.020 - 0.040 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Thermocomp TX88477 PU
LNP* Thermocomp* TX88447 is a compound based on Polyurethane resin containing proprietary fillers.This data was supplied by SABIC-IP for the Americas region.