Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0138 cm/cm | 0.0138 in/in | SABIC Method |
SABIC Innovative Plastics LNP STAT-KON PD000 PA 6 (Europe-Africa-Middle East) LNP* STAT-KON* PD000 is a compound based on PA 6 resin containing Carbon Powder. Added features include: Electrically Conductive. |