Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0074 cm/cm | 0.0074 in/in | 1 hr @ 80°C, flow; SABIC Method |
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS.. |
|||
Linear Mold Shrinkage, Flow | 0.0074 cm/cm | 0.0074 in/in | |
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli.. |
|||
Linear Mold Shrinkage, Flow | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific) LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System. |
|||
Linear Mold Shrinkage, Flow | 0.0074 - 0.0076 cm/cm @Thickness 3.20 mm |
0.0074 - 0.0076 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Linear Mold Shrinkage, Flow | 0.0074 - 0.0076 cm/cm @Thickness 3.20 mm |
0.0074 - 0.0076 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Linear Mold Shrinkage, Flow | 0.0074 - 0.0076 cm/cm @Thickness 3.20 mm |
0.0074 - 0.0076 in/in @Thickness 0.126 in |
SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East) design for black light frame application as high flow PC, V-2, high reflection grade. |
|||
Linear Mold Shrinkage, Flow | 0.0074 cm/cm | 0.0074 in/in | SABIC Method |
SABIC Innovative Plastics LNP THERMOCOMP NX07354 PC+ABS (Asia Pacific) This is a PC/ABS compound, a good candidate for Laser Direct Structuring applications. |
|||
Linear Mold Shrinkage, Flow | 0.0074 cm/cm @Time 86400 sec |
0.0074 in/in @Time 24.0 hour |
ISO 294 |
SABIC Innovative Plastics LNP STAT-KON DX05305C PC LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System. |