1 hr @ 80°C, flow; SABIC Method
SABIC Innovative Plastics SABIC PPCOMPOUND 7450 PP
SABIC® PPcompound 7450 is a mineral filled, impact modified polypropylene TPO. This material can exhibit high impact resistance and good paintability in automotive exterior applications. The IMDS..
Linear Mold Shrinkage, Flow 0.0074 cm/cm
0.0074 in/in
Solvay TECHNYLSTARâ„¢ S 218 MT PA6, 40% mineral filled, DRY
Description: TechnylStar Polyamide, 40% mineral filled, heat stabilized, for injection molding. Characterized by a high fluidity of the melt.Available in: Asia Pacific and North AmericaProduct Appli..
Linear Mold Shrinkage, Flow 0.0074 cm/cm

@Time 86400 sec
0.0074 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX05305C PC (Asia Pacific)
LNP* Stat-kon* DX05305C is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Clean Compounding System.
Linear Mold Shrinkage, Flow 0.0074 - 0.0076 cm/cm

@Thickness 3.20 mm
0.0074 - 0.0076 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC
design for black light frame application as high flow PC, V-2, high reflection grade.
Linear Mold Shrinkage, Flow 0.0074 - 0.0076 cm/cm

@Thickness 3.20 mm
0.0074 - 0.0076 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Asia Pacific)
design for black light frame application as high flow PC, V-2, high reflection grade.
Linear Mold Shrinkage, Flow 0.0074 - 0.0076 cm/cm

@Thickness 3.20 mm
0.0074 - 0.0076 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP Lexan_BFL2200 PC (Europe-Africa-Middle East)
design for black light frame application as high flow PC, V-2, high reflection grade.
Linear Mold Shrinkage, Flow 0.0074 cm/cm
0.0074 in/in
SABIC Method
SABIC Innovative Plastics LNP THERMOCOMP NX07354 PC+ABS (Asia Pacific)
This is a PC/ABS compound, a good candidate for Laser Direct Structuring applications.
Linear Mold Shrinkage, Flow 0.0074 cm/cm

@Time 86400 sec
0.0074 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP STAT-KON DX05305C PC
LNP* STAT-KON* DX05305C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Electrically Conductive, Clean Compounding System.