Polymer Property : Linear Mold Shrinkage, Flow = 0.0046 in/in Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0044 - 0.0046 cm/cm

@Time 86400 sec
0.0044 - 0.0046 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0044 - 0.0046 cm/cm

@Time 86400 sec
0.0044 - 0.0046 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6