Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Linear Mold Shrinkage, Flow = 0.0044 cm/cm Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.0044 - 0.0054 cm/cm

@Thickness 3.20 mm
0.0044 - 0.0054 in/in

@Thickness 0.126 in
SABIC Method
SABIC Innovative Plastics Cycoloy® CY2000 PC+ABS
Cycoloy resin CY2000 is a flame retardant (FR) PC/ABS blend free from halogen containing FR agents. It was designed to meet CA133 application requirements.This data was supplied by SABIC-IP for the ..
Linear Mold Shrinkage, Flow 0.0044 cm/cm

@Thickness 2.00 mm
0.0044 in/in

@Thickness 0.0787 in
ISO 294-4
DuPont Performance Polymers Crastin® SK645FR BK851 PBT  (Unverified Data**)
Crastin® SK645FR BK851 is a flame retardant , 30% glass reinforced black polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.75mm.Information provided by DuPont Performance P..
Linear Mold Shrinkage, Flow 0.0044 cm/cm
0.0044 in/in
Solvay TECHNYL® A 218 V50 PA66, 50% glass fiber, DRY
Description: TECHNYL® A 218 V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Linear Mold Shrinkage, Flow 0.0044 cm/cm
0.0044 in/in
Solvay TECHNYL® C 246 V 30 PA6, 30% glass fiber, DRY
Description: Polyamide PA6, reinforced with 30 % of glass fiber, high impact strength, for injection molding.Available in: Asia Pacific and North AmericaProduct Applications: Having good mechanical ..
Linear Mold Shrinkage, Flow 0.0044 - 0.0046 cm/cm

@Time 86400 sec
0.0044 - 0.0046 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX PA 6
LNP* THERMOCOMP* PH0400CX is a compound based on Nylon 6 resin. Added feature of this grade is: High Specific Gravity.
Linear Mold Shrinkage, Flow 0.0044 - 0.0046 cm/cm

@Time 86400 sec
0.0044 - 0.0046 in/in

@Time 24.0 hour
ASTM D955
SABIC Innovative Plastics LNP THERMOCOMP PH0400CX_BK1D466 PA 6
4.0 specific gravity, Nylon 6
Linear Mold Shrinkage, Flow 0.0044 cm/cm
0.0044 in/in
SABIC Method
SABIC Innovative Plastics LNP Thermocomp PFB42ES PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB42ES is a compound based on PA6 resin containing Glass Fiber, Glass Bead. Added features include: Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-..
Linear Mold Shrinkage, Flow 0.0044 cm/cm

@Thickness 4.00 mm
0.0044 in/in

@Thickness 0.157 in
E2P method
Eurostar Staramide PFB42ES PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42ES is a Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0044 cm/cm

@Thickness 4.00 mm
0.0044 in/in

@Thickness 0.157 in
E2P method
Eurostar Staramide PFB42EU PA6, Glass Fiber/Bead Filled, Injection Molded
Starflam PFB42EU is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar.
Linear Mold Shrinkage, Flow 0.0044 cm/cm
0.0044 in/in
ISO 294-4
Akro-Plastic Akromid® B3 GF 10 (2829) PA 6 Dry, 10% Glass Filled
AKROMID® B (Polyamide 6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperatur..
Linear Mold Shrinkage, Flow 0.0044 cm/cm
0.0044 in/in
60x60x2 mm; ISO 294
BASF Ultradur® FRee B 4440 G5 25% Glass Filled PBT
Description: Is a PBT, injection-molding grade with 25% glass fibers for parts requiring enhanced fire resistance as well as increased tracking resistance (e.g. housings for electronics, plug-and-so..
Linear Mold Shrinkage, Flow 0.0044 cm/cm

@Time 86400 sec
0.0044 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP VERTON RVN17SXS PA 66 (Europe-Africa-Middle East)
LNP* VERTON* RVN17SXS is a compound based on PA 66 resin containing Long Glass Fiber, MoS2. Added features include; Wear Resistant.
Linear Mold Shrinkage, Flow 0.0044 cm/cm
0.0044 in/in
SABIC Method
SABIC Innovative Plastics LNP Thermocomp PFB42EU PA 6 (Europe-Africa-Middle East)
LNP* THERMOCOMP* PFB42EU is a compound based on PA 6 resin containing Glass Fiber, Glass Bead. Added features include Easy Molding, Heat Stabilized.This data was supplied by SABIC-IP for the Europe-..
Copyright © lookpolymers.com All Rights Reserved