Physical Properties | Metric | English | Comments |
---|---|---|---|
Linear Mold Shrinkage, Flow | 0.0015 - 0.0017 cm/cm @Time 86400 sec |
0.0015 - 0.0017 in/in @Time 24.0 hour |
ASTM D 955 |
SABIC Innovative Plastics LNP Stat-kon REL36 PA 66 LNP* Stat-Kon* REL36 is a compound based on Nylon 6/6 containing carbon fiber and PTFE. Characteristics of this grade are Statically Conductive.This data was supplied by SABIC-IP for the Americas r.. |