Physical Properties Metric English Comments
Linear Mold Shrinkage, Flow 0.00070 cm/cm
0.00070 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® AKV 35 CX H2.0 900876 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilizedInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00070 cm/cm
0.00070 in/in
Post-shrinkage, 60x60x2; 120°C; 4 hour; ISO 294-4
Lanxess Durethan® AKV 35 H2.0 SR1 901510 Nylon 66, Glass Fiber Reinforced
PA 66, 35% glass fibers, injection molding, heat-aging stabilized, improved surface finishInformation provided by LANXESS.
Linear Mold Shrinkage, Flow 0.00070 cm/cm

@Time 86400 sec
0.00070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT (Europe-Africa-Middle East)
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.
Linear Mold Shrinkage, Flow 0.00070 cm/cm

@Time 86400 sec
0.00070 in/in

@Time 24.0 hour
ISO 294
SABIC Innovative Plastics LNP Lubricomp WL0049XF PBT
LNP* Lubricomp* WL0049 is a compound based on Polybutylene Terephalate resin containing PTFE and Flame Retardant. Added features include: Internally Lubricated, Flame Retardant.This data was suppl..
Linear Mold Shrinkage, Flow 0.00070 cm/cm

@Thickness 3.17 mm
0.00070 in/in

@Thickness 0.125 in
ASTM D955
Techmer ES Electrablend® ABS CF10 FR BK 10% Carbon Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Carbon Fiber, 10% Filler by WeightFeatures: Flame RetardantAppearance: BlackInformation provided by TP Composites, Inc.
Linear Mold Shrinkage, Flow 0.00070 - 0.00090 cm/cm

@Time 86400 sec
0.00070 - 0.00090 in/in

@Time 24.0 hour
ASTM D 955
SABIC Innovative Plastics LNP Stat-kon AE004E ABS
LNP* Stat-Kon* AE004E is an ABS compound containing Glass Fiber. Characteristics of this grade are Statically Conductive and Easy Molding.This data was supplied by SABIC-IP for the Americas region...
Linear Mold Shrinkage, Flow 0.00070 cm/cm
0.00070 in/in
ASTM D955
Solvay Specialty Polymers Xydar® G-430 Glass Filled Liquid Crystal Polymer  (discontinued **)
XYDAR G-430 Liquid Crystal Polymer (LCP) is a glass reinforced injection molding grade developed specifically for electronic applications utilizing surface mount technology at lead-free solder tempe..
Linear Mold Shrinkage, Flow 0.00070 cm/cm
0.00070 in/in
ASTM D955
Solvay Specialty Polymers Xydar® MG-350 Liquid Crystal Polymer, Mineral and Glass Filled  (discontinued **)<
XYDAR MG-350 Liquid Crystal Polymer (LCP) is a mineral and glass-filled injection molding grade developed specifically for cost-effective performance in applications where a balance of flatness and ..
Linear Mold Shrinkage, Flow 0.00070 cm/cm
0.00070 in/in
Compression molding; ISO 2577
Hexion Bakelite™ PF 4260 Phenolic Formaldehyde Resin, Resistant to High Temperatures, Improved Electrical Properties, Low Shrinkage, High Mechanical Strength
Phenolic molding compound, inorganically filled, glass fiber reinforced, high dimensional stability at raised temperature, good media resistance, heat-resistantApplication areas: Commutators (starte..