Physical Properties | Metric | English | Comments |
---|---|---|---|
c Lattice Constant | 15.12 Ã… | 15.12 Ã… | |
MarkeTech Silicon Carbide (6H) Single Crystal Substrate Data provided by the supplier, MarkeTech International.Developed for deposition of III-V nitrides for LEDs, Lasers, etc. Standard orientation: ; GaN Lattice Mismatch 3.5%. |
|||
c Lattice Constant | 15.12 Å | 15.12 Å | |
Mateck Silicon Carbide Substrate, SiC (6H) Substrate single crystals for III-V nitrides |