Physical Properties Metric English Comments
c Lattice Constant 13.11 Ã…
13.11 Ã…
MarkeTech Lanthanum Aluminum Oxide (LaAlO3) Single Crystal Substrate
Data provided by the supplier, MarkeTech International.Used as a substrate for deposition of high temperature oxide superconductors.
c Lattice Constant 13.11 Ã…
13.11 Ã…
Mateck Lanthanum Aluminate Substrate, LaAlO3 cubic
Substrate single crystals for superconductivity
c Lattice Constant 13.11 Ã…
13.11 Ã…
Mateck Lanthanum Aluminate Substrate, LaAlO3 rhombohedral
Substrate single crystals for superconductivity