Physical Properties | Metric | English | Comments |
---|---|---|---|
Specific Gravity | 0.826 g/cc @Temperature 15.5 °C |
0.826 g/cc @Temperature 59.9 °F |
|
Indium Corp. 3592 Wave Solder Flux, No-Residue 3592 Wave soldering Flux is a low-solids, non-halide rosin/resin free formulation designed to leave a no-residue appearance. This flux contains very effective flux activators that provide excellent.. |