Indium Corp. 3592 Wave Solder Flux, No-Residue

Category Fluid
Manufacturer Indium Corporation of America
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. 3592 Wave Solder Flux, No-Residue.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3592 Wave soldering Flux is a low-solids, non-halide rosin/resin free formulation designed to leave a no-residue appearance. This flux contains very effective flux activators that provide excellent solderability and reduced defects on surface mount, mixed technology and through-hole electronic assemblies.3592 can be used with common board finishes including HASL, Immersion Ag, ENIG, OSP and other alternative coatings to provide excellent through-hole penetration resulting in better topside solder fillets.FeaturesRosin/resin-free with ultra low residue appearanceLow residue won't interfere with probe testing requirementsCan be conformal coated without cleaningMeets IPC and Bellcore reliability specificationsPhysical Properties Color: ClearFlux Type Classification: ORL0Information provided by the manufacturer, Indium Corporation of America.
Physical Properties Metric English Comments
Specific Gravity 0.820 g/cc

@Temperature 25.0 °C
0.820 g/cc

@Temperature 77.0 °F
0.826 g/cc

@Temperature 15.5 °C
0.826 g/cc

@Temperature 59.9 °F
Solids Content 3.0 %
3.0 %
Thermal Properties Metric English Comments
Flash Point 12.2 °C
54.0 °F
TCC
Chemical Properties Metric English Comments
Acid Value 22
22