Specific Gravity 0.793 g/cc

@Temperature 25.0 °C
0.793 g/cc

@Temperature 77.0 °F
Indium Corp. 3577-TF Wave Solder Flux, No-Clean
Wave Solder Flux 3577-TF is a low-solids flux specially formulated to eliminate post-cleaning operations. This flux contains a small amount of resin, which enhances the wetting properties.3577-TF i..
Specific Gravity 0.793 g/cc

@Temperature 15.5 °C
0.793 g/cc

@Temperature 59.9 °F
Indium Corp. 16-1085 Flux Thinner
16-1085 flux thinner is for use with Wave Solder Flux 1085, to maintain specific gravity during use.Physical PropertiesColor: ClearInformation provided by the manufacturer, Indium Corporation of Am..